MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Momentive Performance Materials GE Sealants & Adhesives Ultra Seal Siliconized Acrylic Latex Caulk, White
Categories: Polymer; Thermoset; Silicone

Material Notes: Ultra Seal Siliconized Acrylic Latex caulk is an all-purpose paintable caulk ideal for decorative paint projects where water and moisture may be present. This caulk is paint-friendly and low in odor. It guns out effortlessly, tools smoothly, and cleans-up easily with soap and water. This caulk resists cracking and offers dependable adhesion and flexibility. When fully cured, the caulk is resistant to stain-causing mold and mildew growth and is a great choice for professional results. Guaranteed for as long as you own your home.

Features: Water resistant, Durable and Flexible – exceeds ASTM C-834, 0°C requirements. Strong adhesion to common kitchen and bath building materials including most woods, plaster, masonry, glass, countertops and porcelain tile. Compatible with water or oil-based paints. Low VOC (Meets CARB VOC Limits) and low odor. Easy application. Soap and water clean-up.

Ultra Seal Siliconized Acrylic Latex caulk can be used in a wide variety of interior applications, including trim, cabinets, walls, molding, tiles, and countertops, showers, sinks and tubs.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³Uncured
Solids Content 79 - 83 %79 - 83 %Uncured. % by weight; ASTM C1250
Volatile Organic Compounds (VOC) Content <= 35 g/l<= 35 g/lUncured. Excluding water & exempt compounds
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4444ASTM 661
Elongation at Break 200 %200 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 100 °C104 - 212 °FApplication Temp
Cure Time 1440 min24.0 hour
Tack-Free Time 30.0 min0.500 hourASTM C679
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceSmooth & CreamyUncured
BaseAcrylic Latex
Carb Chem Curing VOC<1.5 wt.%Uncured. Non-Chem Curing.
Clean-upDamp Disposable Cloth
ColorWhiteMAKB210WT 12C
Consistency / SagPassed
Coverage Rate51 Lin. Ft.
Cracking & CaulkingNone-passed
Extension Recovery and Adhesion (Glass/Al.)Passed
Freeze/Thaw StabilityPassed / 5 Cycles at 0°FUncured
Heat Aging and Weight Lost Cracking, CaulkingPassed
Low Temperature FlexibilityPassedASTM C732
OdorSlight AcrylicUncured
Paint Ready Time30 minutes
PaintableLatex & Oil Based Paints
Peel StrengthPassedASTM C794, Dry
Stain/Color ChangePassedASTM C510
Water Ready24 hoursUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9951 / 265763

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.