Hostalen CRP 100 blue is a high density polyethylene (HDPE), blue colored similar RAL 5005 with high melt viscosity for extrusion and injection molding. The product is classified as PE 100 and provides excellent stress crack resistance properties (ESCR) combined with very good long term hydrostatic strength. This grade is not intended for medical and pharmaceutical applications. This grade is supported for use in drinking water applications. Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; South & Central America Application: Drinking Water Pipe Market: Pipe Processing Method: Pipe; Sheet Attribute: Good Creep Resistance; Good ESCR (Environmental Stress Cracking Resistance); Good Organoleptic Properties; Weldable Information provided by LyondellBasell. |