MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman EcoLon® MRGF1619-WBK1 Mineral and Glass Reinforced Recycled Nylon 66  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Post Consumer Nylon Compound; Weatherable

Information provided by Wellman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183-87
Filler Content 19 %19 %
Linear Mold Shrinkage 0.010 - 0.014 cm/cm0.010 - 0.014 in/inISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cm0.010 - 0.014 in/inISO DIS 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 65.0 MPa9430 psiISO 527-93
Elongation at Break 8.0 %8.0 %ISO 527-93
Flexural Strength 100 MPa14500 psiISO 178-93
Flexural Modulus 3.70 GPa537 ksiISO 178-93
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-93

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3L HP PA66 (Dry)
Lotte Advanced Materials Starex® GC-0770 H ABS/PET, Unreinforced Recycled
Lotte Advanced Materials Starex® GC-0710 ABS/PET, Unreinforced Recycled
Lotte Advanced Materials Starex® GC-0703 ABS/PET, Unreinforced Recycled
Celanese Impet® 320R Recycled PET, 15% Glass Reinforced

PWEL740 / 72456

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.