MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Alfa Chemistry Materials Tetrabutylammonium Iodide
Material Notes: Applications: Tetrabutylammonium iodide is used in the preparation of novel quaternary amines to serve as antibacterial agents in the rise of drug-resistant bacteria, it is also used in phosphonium reversible inhibitors of cholinesterases.

Synonyms: FT-0649550; AKOS001093680; ST50508431; CTK3J7262; RTR-031481; Tetrabutylammonium iodide; n-Bu4NI; TRA0077366; (Bu)4NI; AB1002178

Smiles: CCCC[N+](CCCC)(CCCC)CCCC.[I-];

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Molecular Weight 369.189 g/mol"Exact Mass" - Based on Specific Isotopes
 369.189 g/molMonoisotopic Mass - Isotopic Peak from Most Abundant Isotopes
 369.375 g/mol
Storage Temperature <= 30.0 °C
 
Descriptive Properties
Alfa Chemistry Materials CategoryPolymer Science
CAS Number311-28-4
Complexity116
Covalently-Bonded Unit2
EC Number206-220-5
H-Bond Acceptor1
Heavy Atom Count18
InChIInChI=1S/C16H36N.HI/c1-5-9-13-17(14-10-6-2,15-11-7-3)16-12-8-4;/h5-16H2,1-4H3;1H/q+1;/p-1;
InChIKeyDPKBAXPHAYBPRL-UHFFFAOYSA-M;
IUPAC Nametetrabutylazanium;iodide;
Molecular FormulaC16H36IN
NSC Number10414
Rotatable Bond Count12
Topological Polar Surface Area0A^2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ZZALFA2481 / 269051

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.