MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell CirculenRecover PP522H Natural Polypropylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: CirculenRecover PP522H Natural is a clear circular homopolymer supplied in pellet form for the production of biaxially oriented polypropylene films (BOPP). The grade combines a high transparency and a stiffness similar to Moplen HP522H. CirculenRecover PP522H Natural is available in natural color and contains pre-consumer waste. It contains antiblocking agent in the range of 100 to 400 ppm.

Sustainability: According with the requirements of Standard ISO 14021:2016, CirculenRecover PP522H Natural contains, in the development phase from 30% to 35% of recycled material that is based on Pre-Consumer Waste from material diverted from waste stream during the manufacturing process.

This product is not intended for highly regulated applications including food contact, potable water contact, medical and pharmaceutical applications.

Status: Developmental

Availability: Africa-Middle East; Asia-Pacific; Europe

Market: Flexible Packaging

Processing Method: BOPP; Cast Film; Double Bubble

Attribute: High Transparency; Medium Stiffness

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 2.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
Antiblock Level 250 ppm250 ppmNatural Silica
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 71.071.0ISO 868
Tensile Strength at Break 23.0 MPa3340 psiISO 527-1, -2
Tensile Strength, Yield 34.0 MPa4930 psi50 mm/min; ISO 527-1, -2
Elongation at Break >= 500 %>= 500 %50 mm/min; ISO 527-1, -2
Elongation at Yield 12.0 %12.0 %50 mm/min; ISO 527-1, -2
Flexural Modulus 1.45 GPa210 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 155 °C311 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 0.600 %0.600 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9062 / 323997

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.