MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Vycom PROTEC® Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Protec HP is a high corrosion resistant polypropylene material which exhibits excellent tensile strength and stiffness at elevated temperatures. Homopolymer polypropylene possesses excellent resistance to organic solvents and degreasing agents as well as electrolytic attack. Protec has superior working temperatures and tensile strength. In addition, Protec is lightweight, stain resistant and has a low moisture absorption rate.

FEATURES AND BENEFITS

  • Strength- Protec has excellent strength to weight through a range of temperatures.
  • Insulation- Protec has good thermal and electrical insulation properties.
  • Abrasion- Protec has good abrasion resistance and durability.
  • USDA/FDA- Protec is compliant with USDA and FDA regulations for food grade applications.
  • Machinable- Protec can be machined, cut or routed using conventional tooling.
  • Forming- Protec can be thermoformed to make complex parts and shapes.
  • Chemical Resistance- Protec has outstanding chemical compatibility to a broad range of chemistry and temperatures.
  • Purity- Protec is a pure polymer without processing aids or additives.
  • NSF- The National Sanitation Foundation has approved natural Protec HP for food grade contact in food equipment.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 92ASTM D785
Tensile Strength, Yield 5400 psiASTM D638
Elongation at Yield 14 %ASTM D638
Flexural Modulus 225000 psiASTM D790A
Izod Impact, Notched 1.20 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 327 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 210 °FASTM D648
 
Compliance PropertiesOriginal ValueComments
USDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos H07G-00 Polypropylene Homopolymer
Flint Hills P4G3Z-050F Polypropylene Homopolymer
Epsilon Polymers ZP-741 Polypropylene
Celanese Celcon® LW90FS-K POM, Tribological
Carmel Olefins Capilene® G 86 E Polypropylene Homopolymer

PCPCV18 / 29090

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.