MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 24809 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24809 is a very low durometer thermoplastic vulcanizate designed for industrial applications requiring UV resistance. This grade suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Light Stabilized; Low Density; Low Flow; Low Hardness; Low Specific Gravity; Soft; Sunlight Resistant; UV Absorbing; Without Fillers

Uses: Expansion Joint; Gaskets; Glazing; Grommets; Plugs; Rubber Replacement; Shock Absorbing Pads; Tubing; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.892 g/cc0.0322 lb/in³ASTM D792
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  10
@Time 5.00 sec
10
@Time 0.00139 hour
Injection Molded; ASTM D2240
 14
@Time 1.00 sec
14
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 0.827 MPa120 psiFlow, Die C, 20 in/min; ASTM D412
 0.889 MPa129 psiAcross Flow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain  0.303 MPa
@Strain 100 %
44.0 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 0.359 MPa
@Strain 100 %
52.0 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 310 %310 %Flow, Die C, 20 in/min; ASTM D412
 340 %340 %Across Flow, Die C, 20 in/min; ASTM D412
Tear Strength 3.68 kN/m21.0 pliAcross Flow, Die C, 20 in/min; ASTM D624
 4.21 kN/m24.0 pliFlow, Die C, 20 in/min; ASTM D624
Compression Set  10 %
@Temperature 22.8 °C,
Time 79200 sec
10 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395
 24 %
@Temperature 70.0 °C,
Time 79200 sec
24 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 204 °C350 - 400 °FInjection, Melt
Rear Barrel Temperature 149 - 182 °C300 - 360 °FInjection
Middle Barrel Temperature 160 - 182 °C320 - 360 °FInjection
Front Barrel Temperature 166 - 188 °C330 - 370 °FInjection
Nozzle Temperature 177 - 204 °C350 - 400 °FInjection
Zone 1 143 - 166 °C290 - 330 °FExtrusion
Zone 2 149 - 171 °C300 - 340 °FExtrusion
Zone 3 154 - 177 °C310 - 350 °FExtrusion
Zone 4 154 - 177 °C310 - 350 °FExtrusion
Zone 5 154 - 182 °C310 - 360 °FExtrusion
Die Temperature 154 - 177 °C310 - 350 °FExtrusion
Mold Temperature 26.7 - 48.9 °C80.0 - 120 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 40 - 100 rpm40 - 100 rpmInjection
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1195 / 237686

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.