MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay BR® 154 Primer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: BR® 154 is a modified epoxy, corrosion resistant primer developed for use with structural adhesive films demanding continuous mechanical performance at 350°F (177°C) with short time exposure up to 400°F (204°C). It is formulated to provide maximum environmental resistance and durability within the bond line. Articles primed with BR 154 primer and cured have an indefinite shelf life. Primed details should be wrapped in Kraft paper (as protection from dust and dirt) and stored prior to adhesive bonding. Maintaining controlled conditions of 85°F (30°C) maximum temperature and 65% maximum humidity is recommended for extended storage life.

Features & Benefits:

  • Structural properties from -67°F to 400°F (-55°C to 204°C)
  • Compatibility with most 350°F (177°C) service temperature adhesives
  • Protects prepared surfaces from further oxidation
  • Improves hydrolytic stability at the adhesive-to-metal interface

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.871 g/cc
Solids Content 19 - 21 %sprayable
Volatile Organic Compounds (VOC) Content 705 g/l
Storage Temperature <= 29.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °Ccontinuous
 204 °CShort Term
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay BR® 6747-1 Bonding Primer
Northern White Pine Wood
American Pine Wood
Solvay BR® 127 Primer with FM 73 Adhesive
Overview of materials for Thermoset Polyurethane Foam, Unreinforced

PCYTED003 / 180305

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.