MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.11 - 2.20 g/ccAverage value: 1.79 g/cc Grade Count:69
Water Absorption 0.0300 - 0.500 %Average value: 0.136 % Grade Count:24
 0.150 - 0.250 %
@Temperature 50.0 - 50.0 °C
Average value: 0.207 % Grade Count:7
 0.150 - 0.250 %
@Time 173000 - 173000 sec
Average value: 0.207 % Grade Count:7
Viscosity 325 - 1300 cPAverage value: 816 cP Grade Count:9
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cmAverage value: 0.00337 cm/cm Grade Count:32
Spiral Flow 66.0 - 102 cmAverage value: 79.0 cm Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 63.0 - 75.0Average value: 70.2 Grade Count:11
Hardness, Shore D 75.0 - 90.0Average value: 86.5 Grade Count:12
Tensile Strength, Ultimate 50.0 - 2850 MPaAverage value: 314 MPa Grade Count:55
Tensile Strength, Yield 30.0 - 80.0 MPaAverage value: 58.1 MPa Grade Count:8
Elongation at Break 0.600 - 2.04 %Average value: 1.57 % Grade Count:15
Modulus of Elasticity 6.00 - 89.6 GPaAverage value: 21.4 GPa Grade Count:31
Flexural Yield Strength 70.0 - 1200 MPaAverage value: 268 MPa Grade Count:65
 >= 160 MPa
@Temperature 150 - 150 °C
Average value: 249 MPa Grade Count:5
 200 - 375 MPa
@Temperature 130 - 180 °C
Average value: 249 MPa Grade Count:6
 200 - 375 MPa
@Thickness >=1.50 mm
Average value: 249 MPa Grade Count:6
Flexural Modulus 9.60 - 35.0 GPaAverage value: 18.3 GPa Grade Count:56
Compressive Yield Strength 120 - 1000 MPaAverage value: 308 MPa Grade Count:55
Compressive Modulus 7.60 - 46.6 GPaAverage value: 16.7 GPa Grade Count:6
Shear Strength 20.0 - 74.0 MPaAverage value: 46.1 MPa Grade Count:18
Izod Impact, Notched 0.160 - 24.0 J/cmAverage value: 1.71 J/cm Grade Count:17
Izod Impact, Notched (ISO) 60.0 - 300 kJ/m²Average value: 100 kJ/m² Grade Count:9
Izod Impact, Unnotched (ISO) 34.0 - 54.0 kJ/m²Average value: 45.1 kJ/m² Grade Count:9
Charpy Impact Unnotched 0.400 - 6.00 J/cm²Average value: 2.56 J/cm² Grade Count:22
Charpy Impact, Notched 0.150 - 0.800 J/cm²Average value: 0.400 J/cm² Grade Count:14
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 - 5.00e+16 ohm-cmAverage value: 6.28e+15 ohm-cm Grade Count:15
Surface Resistance 1.00e+13 - 1.00e+16 ohmAverage value: 2.01e+15 ohm Grade Count:20
Insulation Resistance 5.00e+7 - 2.00e+15 ohmAverage value: 1.17e+14 ohm Grade Count:21
Dielectric Constant 3.80 - 7.00Average value: 5.04 Grade Count:43
Dielectric Strength 10.0 - 40.0 kV/mmAverage value: 17.3 kV/mm Grade Count:32
 2.7559 - 16.0 kV/mm
@Temperature 90.0 - 90.0 °C
Average value: 9.49 kV/mm Grade Count:3
 2.3622 - 18.0 kV/mm
@Temperature 90.0 - 90.0 °C
Average value: 9.49 kV/mm Grade Count:6
 2.3622 - 18.0 kV/mm
@Thickness 3.00 - 3.00 mm
Average value: 9.49 kV/mm Grade Count:6
Dielectric Breakdown >= 35000 V
@Temperature 90.0 - 90.0 °C
Average value: 31800 V Grade Count:9
 >= 10000 V
@Temperature 90.0 - 90.0 °C
Average value: 31800 V Grade Count:4
 >= 10000 V
@Time 20.0 - 60.0 sec
Average value: 31800 V Grade Count:4
Dissipation Factor 0.00400 - 0.0500Average value: 0.0241 Grade Count:44
Dielectric Loss Index 0.0150 - 0.0320Average value: 0.0210 Grade Count:3
Arc Resistance 170 - 240 secAverage value: 186 sec Grade Count:19
Comparative Tracking Index 180 - 600 VAverage value: 293 V Grade Count:32
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.60 - 92.0 µm/m-°CAverage value: 35.7 µm/m-°C Grade Count:20
 10.0 - 77.4 µm/m-°C
@Temperature 37.8 - 150 °C
Average value: 33.3 µm/m-°C Grade Count:11
Thermal Conductivity 0.0418 - 16.0 W/m-KAverage value: 1.17 W/m-K Grade Count:23
Maximum Service Temperature, Air 130 - 250 °CAverage value: 174 °C Grade Count:17
Deflection Temperature at 0.46 MPa (66 psi) 200 °CAverage value: 200 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 110 - 282 °CAverage value: 216 °C Grade Count:29
Deflection Temperature at 8.0 MPa 100 - 200 °CAverage value: 163 °C Grade Count:11
Glass Transition Temp, Tg 60.0 - 170 °CAverage value: 112 °C Grade Count:16
Flammability, UL94 HB - V-0Grade Count:25
Oxygen Index 38.0 - 50.0 %Average value: 46.0 % Grade Count:3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 - 175 °CAverage value: 163 °C Grade Count:3
Melt Temperature 40.0 - 110 °CAverage value: 76.5 °C Grade Count:5
Mold Temperature 143 - 190 °CAverage value: 170 °C Grade Count:14
Cure Time 0.700 - 3.00 min
@Temperature 150 - 150 °C
Average value: 1.53 min Grade Count:3
Pot Life 20.0 - 120 minAverage value: 92.2 min Grade Count:9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Melamine-Phenolic Copolymer
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for Epoxy, Cast, Unreinforced
Overview of materials for Epoxy Cure Resin
Overview of materials for Epoxy Molding Compound

O1705 / 77890

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.