MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM Cat SR2 Condensation Cure, Styrene Resistant Moldmaking Catalyst
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM Cat SR2 is the standard catalyst for the QM 100 series when casting polyester resins. This is a two-component, room temperature, condensation cure system. The cured rubber has excellent mechanical properties and good shelf-life stability. This is the styrene resistant version of the standard catalysts and is available as QM Cat Blue SR2, QM Cat Purple SR2 and QM Cat Red 3 SR2.

Key Features:

  • Good work life
  • Fast demold time
  • Excellent physical properties
  • Excellent styrene resistance
Main Applications:
  • Molds for polyester resin castings
  • Molds where styrene resistance is required

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccUncatalyzed, QM Cat Blue SR2
 1.00 g/ccUncatalyzed, QM Cat Purple SR2
 1.00 g/ccUncatalyzed, QM Cat Red 3 SR2
Viscosity 100 cPUncatalyzed, QM Cat Blue SR2
 100 cPUncatalyzed, QM Cat Purple SR2
 100 cPUncatalyzed, QM Cat Red 3 SR2
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 - 6.00 hourDemold time, Catalyzed, QM Cat Red 3 SR2
 12.0 - 16.0 hourDemold time, Catalyzed, QM Cat Purple SR2
 16.0 - 24.0 hourDemold time, Catalyzed, QM Cat Blue SR2
Tack-Free Time 0.750 - 1.00 hourCatalyzed, QM Cat Red 3 SR2
 4.00 - 6.00 hourCatalyzed, QM Cat Purple SR2
 6.00 - 8.00 hourCatalyzed, QM Cat Blue SR2
Pot Life 15.0 minCatalyzed, QM Cat Red 3 SR2
 45.0 minCatalyzed, QM Cat Purple SR2
 60.0 minCatalyzed, QM Cat Blue SR2
 
Descriptive Properties
ColorBlueUncatalyzed, QM Cat Blue SR2
 Light blueCatalyzed, QM Cat Blue SR2
 Light purpleCatalyzed, QM Cat Purple SR2
 Light redCatalyzed, QM Cat Red 3 SR2
 PurpleUncatalyzed, QM Cat Purple SR2
 RedUncatalyzed, QM Cat Red 3 SR2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PACC2068 / 199456

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.