MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes:

Features:

  • Excellent barrier properties
  • High stiffness
  • Good processability
  • Low gel
  • Applications:

  • Barrier films
  • Co-extrusion
  • Dry food packaging
  • Information provided by Nova Chemicals

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.960 g/cc0.0347 lb/in³ASTM D792
    Water Vapor Transmission 2.79 g/m²/day0.180 g/100 in²/day
    Oxygen Transmission Rate 1628 cc/m²/day104.8 cc/100 in²/day
    Thickness 38.0 microns1.50 mil
    Melt Flow 1.2 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    1.2 g/10 min
    @Load 4.76 lb,
    Temperature 374 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore D 6969ASTM D2240
    Film Tensile Strength at Yield, MD 25.0 MPa3630 psiASTM D882
    Film Tensile Strength at Yield, TD 23.0 MPa3340 psiASTM D882
    Puncture Energy 0.722 J0.533 ft-lbLow Friction Puncture
    Elmendorf Tear Strength MD 24 g24 gASTM D1922
    Elmendorf Tear Strength TD 450 g450 gASTM D1922
    Dart Drop Test 29.0 g0.0639 lbF50; ASTM D1709/A
    Film Tensile Strength at Break, MD 38.0 MPa5510 psiASTM D882
    Film Tensile Strength at Break, TD 23.0 MPa3340 psiASTM D882
    1% Secant Modulus, MD 839.99 MPa121830 psiASTM D882
    1% Secant Modulus, TD 1270 MPa184200 psiASTM D882
     
    Thermal PropertiesMetricEnglishComments
    Vicat Softening Point 129 °C264 °FASTM D1525
     
    Optical PropertiesMetricEnglishComments
    Haze 41 %41 %ASTM D1003
    Gloss 14 %14 %at 45°; ASTM D2457
     
    Processing PropertiesMetricEnglishComments
    Melt Temperature 200 - 230 °C392 - 446 °F

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    ExxonMobil Hicor® 30 HT 183 OHD Film
    ExxonMobil Hicor® 30 HT 103 OHD Film
    ExxonMobil Hicor® 30 HF 104 OHD Film
    NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin
    NOVA Chemicals Sclair® 99K Homopolymer HDPE Film Resin

    PNOV918 / 54864

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.