SONLOK 3660 is a fast curing; paste like consistency, high strength anaerobic retaining compound for cylindrical fitting parts particularly where bond gaps can approach 0.50mm. This product offers very good gap cure properties. SONLOK 3660 retaining compound is a single component anaerobic adhesive, which develops high strength rapidly when confined in the absence of air between close fitting metal surfaces to prevent loosening and leakage from shock and vibration. Applications: - Ideal to fill gaps up to 0.50 mm diameter clearance.
- Used for restoring correct fits on worn shafts, spun bearings and damaged keyways.
- Excellent retaining, sealing and thread locking compound.
Information provided by Parson Adhesives, Inc. |