MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics TR-2000 Block Insulation
Categories: Ceramic

Material Notes: TR-2000 SL Block Insulation is an asbestos-free insulation, manufactured from calcium silicate and reinforced with cellulose fibers. This item is versatile products available in a wide range of sizes with either beveled or straight edges.

Because of its low conductivity, this board is economical, energy saving insulation. It exhibits minimal shrinkage at top temperature limits, and will not decompose at its maximum service temperature.

Features:

  • Very low thermal conductivity
  • Lightweight
  • Good high-temperature strength
  • Applications:

  • Tub wall insulating material in carbon baking pits
  • Backup insulation in aluminum pot cells
  • Reheat and pusher furnaces
  • General backup insulation
  • Commercial appliances
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.280 g/cc0.0101 lb/in³at ambient temperature
    Loss On Ignition 4.9 %4.9 %
    Porosity 90 %90 %ASTM C493
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.00107 GPa0.155 ksiat ambient temperature
    Compressive Strength 0.0103 MPa
    @Temperature 577 °C
    1.49 psi
    @Temperature 1070 °F
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0800 W/m-K
    @Temperature 260 °C
    0.555 BTU-in/hr-ft²-°F
    @Temperature 500 °F
     0.100 W/m-K
    @Temperature 540 °C
    0.694 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
     0.140 W/m-K
    @Temperature 815 °C
    0.972 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
     0.160 W/m-K
    @Temperature 980 °C
    1.11 BTU-in/hr-ft²-°F
    @Temperature 1800 °F
    Maximum Service Temperature, Air 1050 °C1922 °FContinuous
     1090 °C2000 °FRating
    Shrinkage 1.0 %
    @Temperature 1040 °C
    1.0 %
    @Temperature 1900 °F
    Linear
     
    Component Elements PropertiesMetricEnglishComments
    CaO 46.2 %46.2 %
    Fe2O3 0.30 %0.30 %
    Other 4.9 %4.9 %
    SiO2 48.6 %48.6 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    COI Ceramics Nicalon™ CG SiCO Ceramic Fiber
    Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
    Wacker Silres® MK Powder Silicone Resin
    Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si), Aged
    Sinotek Materials Graphite Sealing Strip Fireproofing Sealing Products

    CTHERM022 / 2342

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.