MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Refractory Composites RS-DR Refractory Sheet
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: TYPE RS-DR is a rigid pre-fired sheet that has been heat-treated to remove all organic binder and is stable to moisture attack. Refractory Sheet Type RS-DR is suited for use as a setter or barrier for use in the sintering of powder metal parts.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.08 g/cc0.0751 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 3.00 GPa435 ksi
Compressive Yield Strength 68.9 MPa9990 psiat 5% compression
 138 MPa20000 psiat 8% compression
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 0.0209 kV/mm0.530 kV/in
Arc Resistance 360 sec360 sec
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.250 J/g-°C0.0598 BTU/lb-°F
Thermal Conductivity 7.78 W/m-K
@Temperature 600 °C
54.0 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Melting Point 1815 °C3299 °F
Maximum Service Temperature, Air 1200 °C2190 °F
Shrinkage 5.0 %
@Temperature 1200 °C,
Time 86400 sec
5.0 %
@Temperature 2190 °F,
Time 24.0 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 90 %90 %
H2O, Water 2.0 %2.0 %depending on humidity
SiO2 10 %10 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-99-45 Refractory Sheet
Zircar Refractory Composites RS-A3 Refractory Sheet
Zircar Refractory Composites RS-99-60 Refractory Sheet
Zircar Refractory Composites RS-A Refractory Sheet
Zircar Refractory Composites RS-A1 Refractory Sheet

CZRCI34 / 2897

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.