MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C66300, H04 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Typical Uses: Clutch discs; Bushings, sleeve; Connectors; Fuse Clips; Switch Gear; Terminals; Fasteners; Lock Washers; Beater bars; Bellows; Diaphragms; Springs; Bridge bearing plates Chemical hardware; Perforated sheets; Textile machinery

Applicable Specifications: Sheet, Strip, Roller Bar & Plate – ASTM B592

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.77 g/cc0.317 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 579 MPa84000 psi
Tensile Strength, Yield 558 MPa81000 psi0.2% Offset
Elongation at Break 17 %17 %
Tensile Modulus 124 GPa18000 ksi
Modulus of Rigidity 47.6 GPa6900 ksi
Poissons Ratio 0.300.30Calculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000690 ohm-cm0.00000690 ohm-cm25% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.9 µm/m-°C
@Temperature 20.0 - 100 °C
9.40 µin/in-°F
@Temperature 68.0 - 212 °F
 17.6 µm/m-°C
@Temperature 20.0 - 200 °C
9.80 µin/in-°F
@Temperature 68.0 - 392 °F
 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
9.90 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 8.93 W/m-K62.0 BTU-in/hr-ft²-°F
Melting Point 999 - 1050 °C1830 - 1920 °F
Solidus 999 °C1830 °F
Liquidus 1050 °C1920 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co <= 0.20 %<= 0.20 %
Copper, Cu 84.5 - 87.5 %84.5 - 87.5 %
Iron, Fe 1.4 - 2.4 %1.4 - 2.4 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P <= 0.35 %<= 0.35 %
Tin, Sn 1.5 - 3.0 %1.5 - 3.0 %
Zinc, Zn 8.9 - 12.6 %8.9 - 12.6 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC66300x5 / 292274

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.