MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Santoprene® 221-64W175 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall or complex profile extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.

  • Recommended for applications requiring excellent flex fatigue resistance.
  • Excellent ozone resistance.
  • Designed for improved UV resistance.
  • Compliant to EU Directive 2003/11/EC regarding marketing and use of certain dangerous substances and preparations, specifically pentabromodiphenyl ether or octabromodiphenyl ether.

Information provided by Advanced Elastomer Systems

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6464.12 in; ASTM D2240
 6969Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 2.555 MPa370.5 psiAir at 302°F, 168 hr; ASTM D573
 6.62 MPa960 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 2.69 MPa390 psiAcross Flow; ASTM D412
Elongation at Break 437 %437 %Air at 302°F, 168 hr; ASTM D573
 460 %460 %Across Flow; ASTM D412
Tear Strength 23.0 kN/m131 pli73°F, Die C; ASTM D624
Compression Set  19 %
@Temperature 22.8 °C,
Time 79200 sec
19 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
 39 %
@Temperature 125 °C,
Time 252000 sec
39 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.42.4ASTM D150
Dielectric Strength 34.3 kV/mm870 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Die Temperature 204 °C400 °FExtrusion
Melt Temperature 177 - 204 °C350 - 400 °FExtrusion
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Back Pressure 5.00 - 20.0 MPa725 - 2900 psiExtrusion
 
Descriptive Properties
ColorNatural Color
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Alcryn® 1060 BK Melt Processable Rubber
A. Schulman Alcryn® 2060 NC Melt Processable Rubber
A. Schulman Alcryn® 2170 BK Melt Processable Rubber
A. Schulman Alcryn® 2160 BK Melt Processable Rubber
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer

PADVA107 / 22797

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.