MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Santex Spring Wire
Categories: Metal; Ferrous Metal; Special-Purpose Steel; Stainless Steel

Material Notes: Sandvik Santex is a high quality stainless steel grade optimal for applications with a high number of cycles where the springs have to retain their mechanical properties under a long period of time. The steel grade has excellent spring properties combined with a high fatigue resistance and a low relaxation rate.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1700 MPa
@Diameter 1.00 - 1.50 mm
 2100 MPa
@Diameter 0.150 - 0.500 mm
Modulus of Elasticity 200 GPaas delivered
 205 GPaas tempered
Poissons Ratio 0.30Calculated
Shear Modulus 77.0 GPaas received
 79.0 GPaas tempered
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.500 J/g-°C
@Temperature 50.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.70 %
Carbon, C <= 0.020 %
Chromium, Cr 17.5 %
Copper, Cu 3.0 %
Iron, Fe 67.7 %as balance
Manganese, Mn 0.85 %
Nickel, Ni 9.4 %
Silicon, Si 0.85 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik 11R51 Spring Wire
Sandvik 9RU10 Spring Wire
Sandvik 12R10 Spring Wire
Sandvik 5R60/5R62 Spring Wire
Sandvik 8R70 Spring Wire

NSANDV274 / 19168

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.