MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Sarcosine Sodium 40% Solution
Categories: Fluid

Material Notes: Formula: C3H6NNaO2

CAS: 4316-73-8

Description: Sarcosine Sodium 40% sol. is a colorless to yellowish liquid, with no odor. It is miscible with water in all proportions.

Synonyms: N-Methylglycine monosodium salt, Sarcosine Sodium Salt, Sodium (methylamino) acetate, Sodium N-methylglycinate

Applications: Intermediate used in the production of Pharmaceuticals, Industrial Chemicals, Textiles and Industry; Also used as a Initial Product for Chemical Synthesis and Corrosion inhibitor

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Molecular Weight 111.1 g/mol111.1 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1.00 - 10.0 °C33.8 - 50.0 °F
Boiling Point 100 °C212 °F
 
Descriptive Properties
Assay39.5 - 40.5%
Color<100APHA, DIN EN 1557

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Suberonitrile
BASF Styropor® P 570 Expandable Polystyrene Additive
BASF Styroclear GH 58 SBC
BASF Pyrrolidine Pure
BASF Propargyl Chloride 35% Solution in Toluene

PBASG1040 / 132673

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.