MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyrocast SC-2600 Refractory Cast Parts
Categories: Ceramic

Material Notes: Resistant to metal and flame abrasion, Pyrocast SC-2600 is the recommended castable refractory for applications such as filter box frames, burner tubes and troughs. The high purity silicon carbide based refractory features high thermal conductivity and good stability at high temperatures.

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.40 g/cc0.0867 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 22.0 MPa3190 psi
Compressive Strength 10.0 MPa1450 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 10.0 W/m-K69.4 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast AR-S Castable Refractory
Pyrotek Pyrocast XL Small Component Refractory
Pyrotek Pyrocast TG Castable Refractory

CPYRO068 / 1807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.