MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives TURBO SEAL SERIES 50 PURPLE FLEXIBLE GASKET SEALANT
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TURBO SEAL SERIES 50 is an anaerobic gasket sealant, which develops medium strength in a short time. The compound cures in the absence of air between close fitting surfaces and will flex with minor flange movements. Provides resistance to low pressure immediately after assembly of flanges.

Applications:

  • Typically used as a form-in-place pump gaskets, thermostats, compressors, transmission housings & axle covers.
  • Thixotropic nature reduces the migration of liquid product after application.

Part Numbers for this data: 50-050, 50-300

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 923-26-2, 15625-89-5, 80-15-9 and 114-83-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Brookfield Viscosity 275000 - 950000 cPRVT Spindle 7 @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 14.0 psi
@Temperature 18.3 - 149 °C
Steel-grit based; ISO 6922
Shear Strength 6.00 MPaISO 4587; Lap, Steel - grit based
 >= 5.00 MPa
@Temperature 22.0 °C,
Time >=86400 sec
ISO 10123; Compressive, Steel pins and collars
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Flash Point >= 93.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.250 - 2.00 hourCure Time, Primed Surfaces
 1.00 - 2.00 hourCure Time, Unprimed Surfaces
 
Descriptive Properties
AppearancePurple
Chemical Resistance100% Initial Strength RetainedAcetone at 22°C, at 500hrs
 15% Initial Strength RetainedGasoline at 22°C, at 1000hrs
 160% Initial Strength RetainedMotor Oil at 125°C, at 500hrs
 165% Initial Strength RetainedMotor Oil at 125°C, at 1000hrs
 20% Initial Strength RetainedGasoline at 22°C, at 500hrs
 80% Initial Strength RetainedWater/Glycol at 87°C, at 500hrs
 80% Initial Strength RetainedWater/Glycol at 87°C, at 1000hrs
 85% Initial Strength RetainedEthanol at 22°C, at 1000hrs
 90% Initial Strength RetainedEthanol at 22°C, at 500hrs
 95% Initial Strength RetainedBrake Fluid at 22°C, at 500hrs
 95% Initial Strength RetainedAcetone at 22°C, at 1000hrs
 95% Initial Strength RetainedBrake Fluid at 22°C, at 1000hrs
CompositionDimethacrylate ester

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML055 / 135209

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.