MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
KKPC KOSYN KBR 720 Polybutadiene Rubber (Low cis BR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polybutadiene Rubber (Low cis BR)

Characteristics: Low cis BR is different in cis content according to the production process and the catalyst. KKPC's low cis LBR has 35% cis content. LBR has high elasticity and reactivity containing about 14% vinyl bond structure. It is used in the tires of motorcycle, footwear, common industrial products, and also utilized as base polymer of HIPS (high impact polystyrene) which is widely used in cabinet of home appliances, interior decoration, and toys. Since these products have high Mooney viscosity and low solution viscosity, it's easier to control rubber particle size and reduce power consumption during processing.

Applications: Footwear, HIPS products, mechanical products

Additional Notes:
cis-1,4 Contents: 33.5%
Volatile Matter: 0.5%
Ash Content: 0.01%
Toluene insoluble gel: 0.01%
Gel Rank: A

This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.

Data provided by Korea Kumho Petrochemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 38 cPViscosity of Solution; 5% Styrene
Mooney Viscosity 35
@Temperature 100 °C
ML1+4
 
Descriptive Properties
Color7APHA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
KKPC KOSYN KBR 710S Polybutadiene Rubber (Low cis BR)
KKPC KOSYN KBR 750 Polybutadiene Rubber (Low cis BR)
Dow SE SLR-4400 Solution polymerized Styrene Butadiene Rubber (S-SBR)
KKPC KOSYN KBR 710H Polybutadiene Rubber (Low cis BR)
KKPC KOSYN KBR 710L Polybutadiene Rubber (Low cis BR)

PKKPC30 / 48761

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.