MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CHT AS5600 Trans RTV, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Description: This is a 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Oxime cure products which are solvent free. It exhibits good primerless adhesion to many substrates especially plastics and cures rapidly at room temperature when in contact with atmospheric moisture. This product can be described as low corrosive but would not be recommended for use with copper or its associated alloys.

Key Features

  • Good adhesion to many substrates
  • Complies with BS5889 type A
  • US Federal TT-S-001543A class A
  • Germany DIN 18540
Application: Applications include but are not limited to, aquarium tunnels, glazing, sealing of lead flashing and sealing of masonry.

Cured Product: 7 days at 23+/-2°C and 60+/-5% humidity

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2828ASTM D2240-95
Tensile Strength 1.12 MPa162 psiISO 37
Elongation at Break 530 %530 %ISO 37
Tensile Modulus 0.000179 GPa0.0260 ksiYoung's
100% Modulus 0.331 MPa48.0 psi
Shear Strength 0.574 MPa83.3 psiLap Shear Aluminum; ASTM D1002
 0.819 MPa119 psiLap Shear Stainless Steel; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 7.00 min0.117 hourTack Free Time / Skin Formation
 720 min
@Temperature 23.0 °C
12.0 hour
@Temperature 73.4 °F
3mm Depth
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
AppearanceThixotropic paste
ColorTranslucent
Cure typeOxime
RheologyPaste
Self BondingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL035 / 314518

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.