MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® T-ION Thermoplastic sheet
Categories: Polymer; Thermoplastic

Material Notes: KYDEX® T-ION is a proprietary thermoplastic sheet with built-in antimicrobial protection, KYDEX ION Technology™, that continuously fights the growth of stain and odor causing bacteria on its surface. Strong disinfectants and cleaners will have no effect due to its superior chemical resistance.

Since KYDEX® T-ION is less hygroscopic than other thermoplastics, it does not require pre-drying, offers superior durability, more uniform forming with less wall thinning and offers significantly greater resistance to a broad range of corrosive chemicals and cleaning solutions. It is available in a wide range of aesthetic choices and is Underwriter’s Laboratories, Inc® recognized Std 94 V-0, 5V. Its KYDEX ION Technology™ is integral to the sheet.

Suggested Application:

  • Aircraft Interiors
  • Mass Transit Vehicle Interior Components
  • Equipment Housings
  • Kiosk Housings
  • Medical Products
Features:
  • Antimicrobial protection inhibits the growth of stain and odor causing bacteria on the sheet surface
  • Antimicrobial protection is integrated into the sheet
  • Antimicrobial protection keeps the surface cleaner between cleanings
  • Available in thicknesses from 0.71mm (0.028”) and up
  • Easy to form with excellent part definition and deep-draw characteristics
  • Recognized by Underwriter’s Laboratories, Inc® for Std 94 V-0, 5V in all thicknesses (testing pending)
  • Form times similar to FR-ABS making it an easy transition from competitive products

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Moisture Absorption 0.0900 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 107ASTM D785
Tensile Strength 49.1 MPaASTM D638
Tensile Modulus 2558 MPaASTM D638
Flexural Strength 72.4 MPaASTM D790
Flexural Modulus 2570 MPaASTM D790
Compressive Yield Strength 54.1 MPaASTM D695
Compressive Modulus 2737 MPaASTM D695
Bearing Yield Strength <= 210 MPaASTM D953
 54.1 MPa
@Strain 4.00 %
ASTM D953
Poissons Ratio 0.382ASTM D638
Shear Strength 44.7 MPaASTM D732
Gardner Impact 51.0 JDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 17.1 kV/mmoil; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.9 µm/m-°CASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 73.6 °Cannealed; ASTM D648
Flammability, UL94 V-0
 
Descriptive Properties
Vertical BurnPass60 and 12 sec; FAR 25.853(a)(i) and FAR 25.853(a)(ii)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSEKIS508 / 325248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.