MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Supreme SAE 10W-30 Synthetic Blend Motor Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Supreme Synthetic Blend Motor Oil is premium quality automotive engine oil.

It is formulated with a combination of synthetic and premium quality conventional base oils and specially selected additives.

Chevron Supreme Synthetic Blend Motor Oil is specially formulated to provide extra protection against harmful engine deposits, while providing excellent oxidation protection and volatility control at extreme temperatures.

Applications

Chevron Supreme Synthetic Blend Motor Oil is recommended for all four-stroke gasoline engines used in passenger cars, light trucks, sports utility vehicles, powerboats, motorcycles, and other mobile and stationary equipment where an API SL or previous API “S” category oil is recommended. It is excellent for high-revving engines in new and higher-mileage small cars and light trucks. It was specially formulated for use in turbocharged engines.

Key Words: CPS Number: 220133; MSDS Number: 8150
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 30.4 °
Viscosity 5800 cP
@Temperature -25.0 °C
Cold Crank
Viscosity Measurement 139Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 71.9 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 10.8 cStASTM D445
Ash 0.90 %Sulfated Ash wt%
 
Chemical PropertiesOriginal ValueComments
Total Base Number 7.5ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -34.0 °CASTM D97
Flash Point 232 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.094 %
Zinc, Zn 0.103 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Inovyn 178GI Polyvinyl Chloride General Purpose - Rigid
Inovyn 260RF Polyvinyl Chloride General Purpose - Rigid
ChevronTexaco Aero 20W-50 Engine Oil AD
ChevronTexaco 940 Gas Engine Oil

WCHEV033 / 74648

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.