MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Röchling SUSTAPEEK® CM CF 30 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Product characteristics:
  • Excellent dimensional stability
  • Flame retardant and self-extinguishing
  • Very low smoke density
Product applications:
  • Seals
  • Oil and Gas Industry
  • Electrical industry

Information provided by Röchling.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³DIN EN ISO 1183-1
Water Absorption 0.10 %0.10 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090DIN EN ISO 868
Tensile Strength, Yield 140 MPa20300 psiDIN EN ISO 527
Elongation at Break 3.0 %3.0 %DIN EN ISO 527
Modulus of Elasticity 10.0 GPa1450 ksiDIN EN ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1e+05<= 1e+05DIN EN 62631-3-1
Surface Resistance <= 1e+05<= 1e+05DIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C13.9 µin/in-°FDIN 53752
Specific Heat Capacity 0.920 J/g-°C0.220 BTU/lb-°FDIN 52612
Thermal Conductivity 0.920 W/m-K6.38 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 343 °C649 °FISO 11357-3
Maximum Service Temperature, Air 250 °C482 °Flong term
 310 °C590 °Fshort term
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling SUSTAPEEK® GF 30 PEEK
Röchling SUSTAPEEK® CF 30 PEEK
Evonik VESTAKEEP® 2000 FC30 PEEK

PROCH9318 / 233020

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.