MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro Baytec® MP-030 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Baytec MP-030 is a diphenylmethane diisocyanate (MDI)-terminated polyether prepolymer based on polypropylene ether glycol (PPG).

Properties / Applications: Baytec MP-030 is a diphenylmethane diisocyanate (MDI)-terminated polyether prepolymer based on polypropylene ether glycol (PPG). It exhibits low viscosity in spite of its low isocyanate content, and can be formulated into one-component moisture-cured binders and sealants and two-component ultrasoft elastomers. Typical applications include rubber crumb binders, flexible caulks, and sealants. As with any product, use of Baytec MP-030 prepolymer in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
 1.02 g/cc
@Temperature 80.0 °C
1.02 g/cc
@Temperature 176 °F
 1.05 g/cc
@Temperature 40.0 °C
1.05 g/cc
@Temperature 104 °F
Viscosity 8000 cP8000 cP
 1000 cP
@Temperature 60.0 °C
1000 cP
@Temperature 140 °F
 4000 cP
@Temperature 35.0 °C
4000 cP
@Temperature 95.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 5.33 MPa773 psiASTM D412
Elongation at Break 617 %617 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °FPMCC
 
Descriptive Properties
AppearanceYellow viscous liquid
Content3.5-4.1%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering E20B Ethylene Propylene Rubber
Polymax® Maxelast® C4807 TPE, Transparent
Polymax® Maxelast® C4800 TPE, Transparent

PCOVEST0248 / 202031

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.