MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC
Categories: Polymer; Thermoset; Composite SMC; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: QC-7753 is a polyester engineered structural composite molding compound that is designed for applications requiring high strength, fire retardant properties, and resistance to elevated temperatures. It offers fast molding cycles and good surface appearance.

  • Form = Rolls, Festooned Sheet
  • Color = Black, Gray
  • Glass Fiber Content = 63% nominal

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.74 g/ccASTM D792
Water Absorption 0.15 %ASTM D570
Linear Mold Shrinkage 0.00050 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 58ASTM D2583
Tensile Strength 220 MPaASTM D638
Flexural Strength 400 MPaASTM D790
Flexural Modulus 15.8 GPaASTM D790
Compressive Strength 172 MPaASTM D695
Shear Modulus 4.50 GPaASTM D4065
Izod Impact, Notched 1600 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air >= 260 °CDeflection Temperature, Load not specified; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 315 °FCompression Molding
Clamp Pressure 400 - 1200 psi
Cure Time 1.25 min
@Thickness 1.52 mm,
Temperature 143 °C
Shelf Life 1.00 Month
@Temperature 23.9 °C
 
Descriptive Properties
Fiber Length (in)1Glass, nominal
FlammabilitySelf ExtinguishingISO 3795

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites QC-8700 63% Glass Fiber Reinforced Vinyl Ester SMC
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC
Quantum Composites QC-8816 66% Glass Fiber Reinforced Polyester Hybrid SMC
Haysite 46000 Polyester SMC, 30% Glass Reinforced

PCOQB901 / 139269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.