MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Vac-Pak® A6200 Fluoropolymer Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Description: Release film. Ideally suited to aerospace applications.

Features & Benefits:

  • High temperature, tough fluoropolymer release film with excellent release characteristics combined with high elongation
  • Suitable for use with all commonly used resin systems
  • Most commonly used in aerospace applications and has numerous OEM approvals
  • Clear blue or red for ease of identification on the cured laminate
  • Available perforated or non-perforated

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12.0 microns0.472 mil
 15.0 microns0.591 mil
 20.0 microns0.787 mil
 25.0 microns0.984 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 41.4 MPa6000 psi
Elongation at Break 350 %350 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
 
Descriptive Properties
ColorBlue and red
Yield10.2 m2/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay VI5
Solvay Stretch-Vac® 3000 Vacuum bagging film
Solvay N1000 Nylon Mesh
Solvay FF03PM PTFE coated glass fabric

PCYTED276 / 180578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.