MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay Chemicals E2000 Methylene chloride
Categories: Fluid; Solvent

Material Notes: Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high volatility is especially recommended to extract materials sensitive towards temperature

EINECS Number: 200-838-9/CAS Number: 75-09-2/UN number: 1593

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.318 - 1.329 g/cc0.04762 - 0.04801 lb/in³D20/4
 1.32 - 1.332 g/cc0.0477 - 0.04812 lb/in³D20/20
 1.288 g/cc
@Temperature 40.0 °C
0.04653 lb/in³
@Temperature 104 °F
 1.297 g/cc
@Temperature 35.0 °C
0.04686 lb/in³
@Temperature 95.0 °F
 1.306 g/cc
@Temperature 30.0 °C
0.04718 lb/in³
@Temperature 86.0 °F
 1.316 g/cc
@Temperature 25.0 °C
0.04754 lb/in³
@Temperature 77.0 °F
 1.325 g/cc
@Temperature 20.0 °C
0.04787 lb/in³
@Temperature 68.0 °F
 1.334 g/cc
@Temperature 15.0 °C
0.04819 lb/in³
@Temperature 59.0 °F
 1.343 g/cc
@Temperature 10.0 °C
0.04852 lb/in³
@Temperature 50.0 °F
 1.352 g/cc
@Temperature 5.00 °C
0.04884 lb/in³
@Temperature 41.0 °F
 1.361 g/cc
@Temperature 0.000 °C
0.04917 lb/in³
@Temperature 32.0 °F
Viscosity  0.30 cP
@Temperature 30.0 °C
0.30 cP
@Temperature 86.0 °F
Dynamic
 0.36 cP
@Temperature 40.0 °C
0.36 cP
@Temperature 104 °F
Dynamic
 0.38 cP
@Temperature 35.0 °C
0.38 cP
@Temperature 95.0 °F
Dynamic
 0.41 cP
@Temperature 25.0 °C
0.41 cP
@Temperature 77.0 °F
Dynamic
 0.43 cP
@Temperature 20.0 °C
0.43 cP
@Temperature 68.0 °F
Dynamic
 0.46 cP
@Temperature 15.0 °C
0.46 cP
@Temperature 59.0 °F
Dynamic
 0.48 cP
@Temperature 10.0 °C
0.48 cP
@Temperature 50.0 °F
Dynamic
 0.51 cP
@Temperature 5.00 °C
0.51 cP
@Temperature 41.0 °F
Dynamic
 0.53 cP
@Temperature 0.000 °C
0.53 cP
@Temperature 32.0 °F
Dynamic
Molecular Weight 84.9 g/mol84.9 g/mol
Vapor Pressure  0.189 bar
@Temperature 0.000 °C
142 torr
@Temperature 32.0 °F
 0.241 bar
@Temperature 5.00 °C
181 torr
@Temperature 41.0 °F
 0.304 bar
@Temperature 10.0 °C
228 torr
@Temperature 50.0 °F
 0.379 bar
@Temperature 15.0 °C
284 torr
@Temperature 59.0 °F
 0.469 bar
@Temperature 20.0 °C
352 torr
@Temperature 68.0 °F
 0.575 bar
@Temperature 25.0 °C
431 torr
@Temperature 77.0 °F
 0.700 bar
@Temperature 30.0 °C
525 torr
@Temperature 86.0 °F
 0.847 bar
@Temperature 35.0 °C
635 torr
@Temperature 95.0 °F
 1.016 bar
@Temperature 40.0 °C
762.1 torr
@Temperature 104 °F
 
Descriptive Properties
AppearanceClear without suspended matterASMT D3741/B
Color<10APHA
Composition<1 mg/kgOxidizing Compounds (Cl2)
 <1 mg/kgHeavy Metals* (Pb)
 <100 mg/kg1,2-Dichloroethane
 <100 mg/kg1,1-Dichloroethylene
 <12 mg/kgCarbon Tetrachloride
 <5 mg/kgAcidity (HCl)
 <50 mg/kgMoisture (H2O), Karl Fischer, ASTM E1064
 <56 mg/kgChloroform
 1500-2500 mg/kgStabilizer (Ethanol)
Purity>999.5 g/kgwithout stabilizers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dichloromethane (CH2Cl2; Methylene Chloride)

WSOLV143 / 147792

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.