MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) TOLCIDE® PS24DF Surfactant
Categories: Fluid

Material Notes: Standard Applications: TOLCIDE® PS24DF has been specifically developed for use in the treatment of inorganic slurries, color coatings and drilling fluids, whereby it provides effective microbial control without affecting the viscosity or rheology of the treated product. TOLCIDE® PS24DF is particularly suitable for the treatment of calcium carbonate slurries, giving effective protection from microbial spoilage whilst maintaining optimum pumpability of the slurry. Formulations of the TOLCIDE® PS24DF type are Rhodia/Solvay patented technology (International Patent Application WO 2004/066731).

Identification: Proprietary formulation based upon Tetrakishydroxymethyl Phosphonium Sulphate (THPS) formulated with a dispersing agent.

CAS No: 55566 – 30 – 8

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 - 1.29 g/ccOSTM059
pH 3.0 - 6.0OSTM056
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear, yellow to pale pink
Content<15 NTUTurbidity, OSTM064
 22-24%Assay, OPTI03

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY877 / 218605

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.