MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ LUBRICOMP™ Compound ZL003 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: LNP LUBRICOMP ZL003 compound is based on Polyphenylene Ether / Polystyrene (PPE/PS) blend containing 15% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D792
 1.15 g/cc0.0415 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/in24hrs; ASTM D955
 0.0083 cm/cm0.0083 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0087 cm/cm0.0087 in/in24hrs; ISO 294
 0.0090 cm/cm0.0090 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.0 MPa6670 psiASTM D638
 48.0 MPa6960 psiISO 527
Tensile Strength, Yield 47.0 MPa6820 psiASTM D638
 48.0 MPa6960 psiISO 527
Elongation at Break 8.3 %8.3 %ISO 527
 8.9 %8.9 %ASTM D638
Elongation at Yield 8.1 %8.1 %ISO 527
 8.5 %8.5 %ASTM D638
Tensile Modulus 2.06 GPa299 ksi50 mm/min; ASTM D638
 2.25 GPa326 ksi1 mm/min; ISO 527
Flexural Strength 75.0 MPa10900 psiASTM D790
 75.0 MPa10900 psiISO 178
Flexural Modulus 2.00 GPa290 ksiISO 178
 2.75 GPa399 ksiASTM D790
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
Izod Impact, Unnotched 2.67 J/cm5.00 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 17.0 kJ/m²8.09 ft-lb/in²80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.280.28ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.200.20ASTM D3702 Modified: Manual
K (wear) Factor 22.2 x 10-8 mm³/N-M11.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 128 °C
@Thickness 3.20 mm
262 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 119 °C246 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 117 °C
@Thickness 3.20 mm
243 °F
@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 290 - 300 °C554 - 572 °F
Zone 3 300 - 310 °C572 - 590 °F
Melt Temperature 300 - 305 °C572 - 581 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81117 / 289064

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.