MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crosspolimeri FRAGOM PR/04 AFKK N NAT UV HFFR
Categories: Polymer; Thermoset

Material Notes: FRAGOM: is our HFFR thermoplastic compound low flame propagation in fire conditions PVC free and heavy-metal free.

FRAGOM PR/04 AFKK N NAT UV: it is studied to extrude sheathing of telephone cables with aluminum tape at high speed, Compound without migration risks (plasticizers-free). Suitable for sheathing extrusion of cables with size > 60 mm2.

Certify: CEI2011 M1, VDE0207HM4(K=0,7), BS7655 LTS 3-4

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 21.6 kg,
Temperature 160 °C
8.0 g/10 min
@Load 47.6 lb,
Temperature 320 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength >= 12.0 MPa>= 1740 psiIEC 60811
 >= 15.0 MPa
@Temperature 110 °C,
Time 605000 sec
>= 2180 psi
@Temperature 230 °F,
Time 168 hour
Heat Ageing; IEC 60811
Elongation at Break >= 170 %>= 170 %IEC 60811
 >= 212.5 %
@Temperature 110 °C,
Time 605000 sec
>= 212.5 %
@Temperature 230 °F,
Time 168 hour
Heat Ageing; IEC 60811
Tear Strength >= 10.0 kN/m>= 57.1 pliBS 6469-99-1
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 90.0 °C
@Time 21600 sec
194 °F
@Time 6.00 hour
<40%, Penetration (K=0,7); IEC 60811
Smoke Density <= 8.0 min<= 8.0 minflaming mode; ASTM E662
 <= 13 min<= 13 minno flaming mode; ASTM E662
Oxygen Index 30 %30 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 130 °C266 °F
Zone 2 145 °C293 °F
Zone 3 160 °C320 °F
Zone 4 180 °C356 °F
Die Temperature 190 °C374 °F
Head Temperature 185 °C365 °F
Dry Time  3.00 hour
@Temperature 80.0 °C
3.00 hour
@Temperature 176 °F
 4.00 hour
@Temperature 90.0 °C
4.00 hour
@Temperature 194 °F
 
Descriptive Properties
Conductivity<4 µS/mmIEC 60754-2
Corrosivity of gases evolved>4,5 pHIEC 60754-2
Halogen Content0IEC 60754-1
Smoke emission>60%IEC 61034-2
Temperature Index Value>300°C21% O2, NES 715
UV ResistanceNo Crack720h, HD 605/A1 2.4.20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS080 / 294164

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.