MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Epsan Eplamid 66 NC LN K B4 Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: An unreinforced polyamide 66, externally lubricated for injection molding and extrusion application. Eplamid 66 NC LN K B4 offers all of primary properties of unreinforced polyamide 66.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Water Absorption 1.3 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.013 cm/cmParallel; ISO 294-4
 0.017 cm/cmNormal; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 70.0 MPaISO 527-2
Elongation at Break 50 %ISO 527-2
Tensile Modulus 2900 MPaISO 527-2
Flexural Strength 98.0 MPaISO 178
Flexural Modulus 3000 MPaISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²ISO 180/1A
Charpy Impact, Notched 4.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VEN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 205 °CISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75-2/A
Vicat Softening Point 240 °CISO 306/B50
Flammability, UL94 V-2
@Thickness 1.60 mm
EN 60695-11-10
Glow Wire Ignition Temperature 700 °C
@Thickness 0.800 mm
EN 60695-2-13
 700 °C
@Thickness 1.60 mm
EN 60695-2-13
 700 °C
@Thickness 3.00 mm
EN 60695-2-13
Glow Wire Flammability Index 850 °C
@Thickness 0.800 mm
EN 60695-2-12
 850 °C
@Thickness 1.60 mm
EN 60695-2-12
 850 °C
@Thickness 3.00 mm
EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 °CRecommended Injection Molding Temperature
Drying Temperature 80.0 °CAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEPSAN090 / 186404

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.