MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BP Amoco Fortilene® SG6812 Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Produced by gas phase polymerization. This reactor-made thermoplastic olefin is intended for automotive applications that require excellent processability and very high impact resistance at low temperatures. Meets FDA requirements of 21 CFR 177.1520 and is approved by U.L. for their 94HB-flammability rating.

Information provided by Solvay Polymers.

This product is not listed in the standard Innovene product line. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortilene® Polypropylene product line from Solvay Polymers in November 2001.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.895 g/ccASTM D1505
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM D2240
Tensile Strength, Yield 20.7 MPa2 in/min; ASTM D638
Elongation at Yield 10 %2 in/min; ASTM D638
Flexural Modulus, 1% Secant 0.897 GPa0.05 in/min; ASTM D790
Izod Impact, Notched 0.530 J/cm
@Temperature -30.0 °C
ASTM D256
 5.30 J/cm
@Temperature 23.0 °C
ASTM D256
Gardner Impact 23.6 J
@Thickness 3.17 mm,
Temperature -20.0 °C
Test method CLP 463DB-14-01, 8 lb dart
Impact Test 30.0 J
@Thickness 2.00 mm,
Temperature 0.000 °C
Instrumented dart impact (Dynatup) at 0°C. Energy at break, 20mm tup, 50lb, 1m impact on 2mm thick part. ISO 6603
 
Thermal PropertiesOriginal ValueComments
Melting Point 161 °CASTM 3418
Crystallization Temperature 115 °CASTM 3418
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °CASTM D648
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLMR / 68306

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.