Hostacom TRC 452N is a 20% talc filled PP copolymer, with excellent impact/stiffness balance and good flowability and good scratch resistance, outstanding blooming resistance at elevated temperatures and good antistatic behavior. Product is available as a customized color matched, pellet form. This grade is delivered in G72758 color version. Applications: Automotive Parts, Instrument Panels, Interior TrimsInformation provided by LyondellBasell. |