MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Tra-Con Tra-Bond FS279 Blush-Free Non-Sag Structural Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND FS-279 is a two-part epoxy adhesive specifically formulated to be non-sagging and have improved adhesion to smooth, non-porous substrates such as glass, ceramic, stainless steel, etc. This formulation has structural reinforcements which enhance its overall physical characteristics making it ideal for structural bonding applications. Fully cured TRA-BOND FS-279 provides excellent resistance to salt solutions, mild acids and alkalis and many other chemicals including petroleum solvents, lubricating oils and alcohols.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccMixed
Viscosity 375000 cP
@Temperature 25.0 °C
375000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C
@Temperature 20.0 °C
30.6 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.0 °C
1.00 - 2.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 60 min60 min
 
Descriptive Properties
Color Milky, Translucent
Mix Ratio, parts by weight100/39Resin/Hardener
Thixotropic Index 5.85 rpm/50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC276 / 71204

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.