MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 1500-55D TFE 15 Polyether-Ester Block Copolymer (TEEE / COPE), PTFE Lubricated
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D 792
Filler Content 15 %Primary Additive
Linear Mold Shrinkage 0.015 - 0.025 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55instantaneous; ASTM D 2240
Tensile Strength at Break 3700 psi
@Thickness 3.20 mm
Type I; 0.2 in/min (5 mm/min); ASTM D638
Elongation at Break >= 500 %
@Thickness 3.20 mm
Type I; 0.2 in/min (5 mm/min); ASTM D638
Tensile Modulus 40.0 ksiASTM D 638
Flexural Strength 1600 psi
@Thickness 3.17 mm
5% Strain; 0.05 in/min (1.2 mm/min); ASTM D790
Flexural Modulus 40.0 ksiASTM D 790
Izod Impact, Unnotched NB
@Thickness 3.17 mm
ASTM D4812
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 410 - 460 °F
Mold Temperature 70.0 - 120 °F
Drying Temperature 220 °F
Dry Time 2 - 4 hour
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1501-40D Polyether-Ester Block Copolymer (TEEE / COPE); Glass Fiber
RTP Company RTP 1500-40D UV NATURAL Polyether-Ester Block Copolymer (TEEE / COPE), UV Stabilized
RTP Company PermaStat® 1500-50D Polyether-Ester Block Copolymer (TEEE/COPE), Permanently Anti-static - ESD Protection
RTP Company RTP 1500-55D TFE 10 Polyether-Ester Block Copolymer (TEEE/COPE), PTFE Lubricated
Fluorocarbon Rubber (FPM), Low Temperature Grade

PQZWA12773 / 90732

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.