Hostacom HBG 2266L NAT is a glass fiber reinforced PP homopolymer with low melt flow rate. Product is not UL certified. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: White Goods Market: Electrical / Electronics Processing Method: Injection Molding Information provided by LyondellBasell. |