MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials MEGUM™ W 9700 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: One-component waterborne adhesive for bonding castable urethane or nylon to metal or other solid materials.

Information provided by DuPont Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D 4052
Density 1.10 g/ccISO 1183
 1.75 g/ccDry Film
Solids Content 20 - 24 %
pH 6.0 - 8.0
Viscosity 50 - 300 cP
Thickness 10.0 - 20.0 micronsRecommended film thickness
 
Processing PropertiesOriginal ValueComments
Dry Time 0.250 - 0.500 hour
Shelf Life 12.0 Month
 
Descriptive Properties
ColorBlack
CompatibilityMetals
 Rubber
Dilutionundiluted to 0.25
 undiluted, brushing
 undiluted, dipping
Oven pre-bake temperature80Oven pre-bake temperature, 6 hr.
PolymerAdhesive
Regional AvailabilityEurope
 Near East/Africa
Solvent or thinnerdeionized or distilled water
Theoretical coverage (m²/L)5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDTF9304d / 295976

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.