MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
ALM PA 250 Nylon 12 SLS Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Highly Recyclable Nylon 12 Laser Sintering Material.

Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or no scrap material, with typical virgin refresh rates from 15 to 25%. Good temperature control is required to process this material.

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 g/ccASTM D1895
Density 1.01 g/ccSintered Part; ASTM D792
Particle Size 30 - 50 µmRange (D10 to D90); Laser Diffraction
 40 µmAverage D50; Laser Diffraction
Melt Flow 40 g/10 min
@Load 5.00 kg,
Temperature 235 °C
3 min.; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 46.0 MPaXY direction; ASTM D638
Tensile Strength, Ultimate 36.0 MPaZ direction; ASTM D638
Elongation at Break 4 %Z direction; ASTM D638
 16 %XY direction; ASTM D638
Tensile Modulus 2.14 GPaZ direction; ASTM D638
 1740 MPaXY direction; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.1e+14 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Melting Point 181 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 179 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °CASTM D648
 
Descriptive Properties
ColorBlack
Surface Finish9 microns

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Overview of materials for Nylon 12
ALM PA 860 White Nylon 11 SLS Prototyping Polymer
3D Systems DuraForm® PA Nylon for SLS® Systems
ALM D80-ST Nylon 11 SLS Prototyping Polymer

PALAP990 / 176049

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.