MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Plansee DENAL® 917 108 XXX (1) Tungsten-Nickel-Iron-Cobalt Alloy
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Characteristics:
  • exceptionally strong
  • high density
  • outstanding mechanical damping capabilities
  • High absorption of X-ray and gamma radiation

Information provided by Plansee.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 17.55 g/cc17.55 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1255 - 1315 MPa182000 - 190700 psi
Tensile Strength, Yield 1220 - 1280 MPa177000 - 186000 psi
Elongation at Break 8.5 - 12 %8.5 - 12 %
Charpy Impact, Notched 105 - 170 J/cm²500 - 809 ft-lb/in²
 
Component Elements PropertiesMetricEnglishComments
Other, total 2.5 - 10 %2.5 - 10 %Ni + Fe + Co
Tungsten, W 90 - 97.5 %90 - 97.5 %
 
Descriptive Properties
Ductilitymuch greater than pure W
Fineness of Graingreater than pure W
Machinability/Workabilitymuch greater than pure W

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plansee DENAL® 920 60 20 Tungsten-Nickel-Iron-Cobalt Alloy
Plansee DENAL® 910 179 20 Tungsten-Nickel-Iron-Cobalt Alloy
Plansee DENAL® 920 159 20 Tungsten-Nickel-Iron-Cobalt Alloy
Plansee DENAL® 917 108 XXX (2) Tungsten-Nickel-Iron-Cobalt Alloy
Overview of materials for Stainless Steel

NPLAM950 / 135506

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.