MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Primex Plastics Prime Co Faraprene-200 Thermoplastic Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Prime Co Faraprene 200, a proprietary compound, provides the benefits of thermoplastic rubber without the odor associated with comparable products. You will benefit from this ABA constructed product that features two prime sides for a pleasing look and feel, and a core layer that provides exceptional flexibility. This pliable composition reduces “set” issues associated with folding or bending when shipped and is favored in packaging applications. Cost and adaptable processing make this sheet a fit for a variety of applications.

Applications: Prime Co Faraprene200’s durability, low cost, and aesthetics are ideal for use in automotive floor mat applications and well suited for marine, cargo trailers, and RVs.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.986 g/ccASTM D792
Melt Flow 0.499 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D2240
Hardness, Shore D 45ASTM D2240
Film Elongation at Break, MD 843 %ASTM D412
Film Elongation at Break, TD 795 %ASTM D412
Tear Strength 486 pliTD; ASTM D624
 505 pliMD; ASTM D624
Film Tensile Strength at Break, MD 1600 psiMax; ASTM D412
 1300 psi
@Strain 100 %
ASTM D412
Film Tensile Strength at Break, TD 1640 psiMax; ASTM D412
 1320 psi
@Strain 100 %
ASTM D412
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness >=1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRIM014 / 278485

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.