MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain Chemlam® 3320 Multi-plied, Flexible, Non-porous Fluoropolymer Laminated Composite
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Chemlam® Ultra® is the trademark for the Chemfab® family of multi-plied, flexible, non-porous fluoropolymer laminated composites that combine the feature of multi-layer fluoropolymer cast films with the mechanical properties of fiber glass reinforced fabric. The Ultra® product line offers high performance in severe thermal cycling, chemical applications.
FEATURES:
PTFE cast barrier film surface, crack and pinhole free:
Outperforms simple PTFE-coated materials; long-lasting release properties make cleaning easier; low wicking of product into fabric extends useful life.
Uniform film thickness over entire surface: Lamination eliminates the possibility of thin spots found in coated materials, which often lead to their premature failure.
Thick gauge films with hardened surfaces: Extended abrasion and wear properties result in longer life with less maintenance.
High temperature, multi-ply fabrics: Exceptional mechanical properties and dimensional stability at any thickness due to the "plywood" effect; designed for thermal cycling and harsh chemical applications, including cooking and plastic processing.
FDA Compliant: Suitable for use in direct food contact applications under the applicable requirements of 21CFR177.1550. All data based on a 0.011 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.063 g/cc2.063 g/ccWoven Density
 
Mechanical PropertiesMetricEnglishComments
Tear Strength Test 4.04.0Lbs./In. Propagation Tear Strength in fill/transverse direction
 7.07.0Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 40.3 kN/m230 pliFill/Transverse direction
 57.8 kN/m330 pliWarp/Longitudinal direction
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorBrown/Black
Weight (oz/yd^2)17

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQZ227 / 68741

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.