Halogen-free, radiation cross-linkable, flame retardant sheathing compound for power and telecommunication cables Compound class: Sheathing Compound category: RDX Flame retardant: ATH Standards: DIN EN 50264 EM101-104; IEC 60092-360 SHF 2; NEK 606 Typical applications: Halogen-free, low smoke, highly oil and extra fuel resistant radiation cross-linkable, flame retardant compound for thin wall insulation of wire for Rolling Stock, Offshore and Marine/Aerospace applications. Features: Flame retardant; Halogen-free; Low smoke; Oil resistant; High temperature resistant Information provided by Melos |