MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® LR 34004/50 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® LR 34004/50 A/B is a paste-like, white two-component liquid silicone rubber with a very short curing time. Vulcanizates are noted for their radio paqueness.

Special features: ELASTOSIL® LR 34004/50 A/B contains barium sulfate as a radio-opaque additive which meets the requirements of the US and European Pharmacopoeia.

Application: ELASTOSIL® LR 34004/50 A/B is particularly suitable for the economical production of large series of injection-molded articles. ELASTOSIL® LR 34004/50 A/B is designed for medical and pharmaceutical applications including implantation for < 30 days.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³DIN EN ISO 1183-1 A
Viscosity 980000 cP
@Shear Rate 0.900 1/s
980000 cP
@Shear Rate 0.900 1/s
DIN EN ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050DIN 53505
Tensile Strength at Break 6.90 MPa1000 psiDIN 53504 S1
Elongation at Break 420 %420 %DIN 53504 S1
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
Postcuring 4h/200°C
 
Descriptive Properties
Appearancewhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9180 / 204709

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.