System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
DuPont Mobility and Materials Zytel® EFE7374 BK416 PA6-IGF40
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 40% Glass Fiber Filled
Material Notes:
40% Glass Reinforced, Toughened, Polyamide 6
While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.41
g/cc
DAM; ISO 1183
Water Absorption
5.4 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption
1.70 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow
0.0020
cm/cm
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.0060
cm/cm
DAM; ISO 294-4, 2577
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
130
MPa
50% RH; ISO 527-1/-2
190
MPa
DAM; ISO 527-1/-2
Elongation at Break
3.5 %
DAM; ISO 527-1/-2
7.5 %
50% RH; ISO 527-1/-2
Tensile Modulus
7500
MPa
50% RH; ISO 527-1/-2
12000
MPa
DAM; ISO 527-1/-2
Poissons Ratio
0.33
DAM; ISO 527-1/-2
0.34
50%RH; ISO 527-1/-2
Izod Impact, Unnotched (ISO)
18.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
19.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
24.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
30.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched
105
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
110
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
113
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
118
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched
17.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
18.0
kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
24.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
33.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Thermal Properties
Original Value
Comments
Melting Point
221
°C
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi)
212
°C
DAM; ISO 75-1/-2
Flame Spread
33.0
mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Processing Properties
Original Value
Comments
Melt Temperature
260
-
280
°C
Injection
270
°C
Injection Optimum
Mold Temperature
50.0
-
90.0
°C
Injection
100
°C
Injection Optimum
Drying Temperature
80.0
°C
Injection
Dry Time
2.00
-
4.00
hour
Dehumidified Dryer; Injection
Moisture Content
0.20 %
Injection
Hold Pressure
50.0
-
100
MPa
Injection
Descriptive Properties
Delivery form
Pellets
Drying Recommended
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
Hold pressure time (s/mm)
3
Injection
Max. screw tangential speed (m/s)
0.2
Injection
Part Marking Code
PA6-IGF40
ISO 11469
Processing
Injection Molding
Regional Availability
Europe
Near East/Africa
Resin Identification
PA6-IGF40
ISO 1043
Special characteristics
Heat stabilized or stable to heat
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 73G40T BK416 PA6-IGF40
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)
Celanese Nilit FRIANYL B63 HS-GV40 Nylon 6 for injection molding, 40% glass fiber reinforced
DuPont Mobility and Materials Zytel® EFE1068 NC010T PA66
Plastcom SLOVAMID 6 GF 40 Polyamide 6, 40% Glass Fiber
PDSX5393 / 198033
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.