MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Moly Low Temp NGLI Grade 1
Categories: Fluid; Lubricant; Aluminum Gellant

Material Notes: Moly Low Temp is a multipurpose, extreme-pressure (EP) aluminum complex grease developed for use in automotive and industrial equipment operating at low ambient temperatures down to -40°F. It has good mobility at low temperatures plus a high dropping point for year-round use in arctic climates. Moly Low Temp is manufactured with low-viscosity base oils and an aluminum complex soap thickener. It is compounded with select additives that provide extreme-pressure and antiwear properties, good oxidation resistance, and rust and corrosion protection. It is fortified with 5% molybdenum disulfide (moly) for extra protection in equipment subject to heavy or shock loads. It has good shear stability and resistance to water washout. It is suitable for both winter and summer use in arctic climates.

Applications:

  • Mobile equipment and industrial machinery operating for prolonged periods at temperatures substantially below 32°F
  • Chassis parts, wheel bearings, spring shackles and king pins on automotive and other mobile equipment operating in arctic climates
  • Chassis parts and wheel bearings on mobile equipment such as lift trucks operating in refrigeration plants, cold storage rooms and sharp-freeze rooms
  • Plain and rolling-element bearings, slides and linkages on industrial equipment operating in cold rooms or at low ambient temperatures
  • Track roller bearings and chassis parts on tractors, coal haulers, snow removal equipment and other heavy equipment operating in cold climates
Features/Benefit:
  • Suitable for year-round use in mobile equipment and industrial machinery operating in arctic climates
  • Good low-temperature properties down to -40°F
  • Good extreme-pressure and antiwear properties
  • Contains moly for extra protection under heavy or shock loads
  • Good oxidation resistance
  • Protects against rust and corrosion
  • Good shear stability
  • Good resistance to water washout

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.68 lb/gal
Viscosity Measurement 58Index
Saybolt Viscosity at 100°F 130 SUS
Saybolt Viscosity at 210°F 40.7 SUS
Kinematic Viscosity at 40°C (104°F) 25 cSt
Kinematic Viscosity at 100°C (212°F) 4.3 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Penetration 310 - 340
Timken Test 45.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 149 °C
Minimum Service Temperature, Air -40.0 °C
Dropping Point 260 °C
 
Descriptive Properties
ColorGray-black
Composition5%Molybdenum Disulfide
ThickenerAluminum Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5126 / 198379

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.