MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Entec Enflex® S3040AE Styrenic Block, TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Product Description: 40 Shore A TPE (Styrenic Block Copolymer based) for extrusion applications, offering soft/tactile fell, grumpiness, and adhesion (Co-Extrusion) to Polypropylene.

Availability: North America

Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Adhesion; Good Colorability; Good Processability; High Elasticity; Low Compression Set; Oil Resistant; Ozone Resistant; Recyclable Material; Soft; Solvent Resistant; UV Resistant

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  36
@Time 10.0 sec
36
@Time 0.00278 hour
Extruded; ASTM D2240
 38
@Time 10.0 sec
38
@Time 0.00278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 4.14 MPa601 psiASTM D412
Tensile Stress 0.758 MPa
@Strain 100 %
110 psi
@Strain 100 %
ASTM D412
Elongation at Break 800 %800 %ASTM D412
Tear Strength 20.2 kN/m115 pliASTM D624
Compression Set  16 %
@Temperature 22.8 °C,
Time 79200 sec
16 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395B
 55 %
@Temperature 70.0 °C,
Time 79200 sec
55 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -65.0 °C-85.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 177 °C320 - 350 °FHopper, Extrusion
Rear Barrel Temperature 171 - 199 °C340 - 390 °F
Middle Barrel Temperature 177 - 210 °C350 - 410 °F
Front Barrel Temperature 191 - 221 °C375 - 430 °F
Nozzle Temperature 199 - 229 °C390 - 445 °F
Zone 1 171 - 191 °C340 - 375 °F
Zone 3 179 - 199 °C355 - 390 °F
Zone 5 191 - 210 °C375 - 410 °F
Adapter Temperature 191 - 210 °C375 - 410 °F
Die Temperature 191 - 210 °C375 - 410 °F
Melt Temperature 191 - 199 °C375 - 390 °FExtrusion
 199 - 221 °C390 - 430 °FInjection
Mold Temperature 10.0 - 48.9 °C50.0 - 120 °FInjection
Drying Temperature 65.6 - 71.1 °C150 - 160 °FInjection
 65.6 - 71.1 °C150 - 160 °FExtrusion
Injection Pressure 5.17 - 8.96 MPa750 - 1300 psi
Cushion 0.508 - 1.27 cm0.200 - 0.500 in
Screw Speed 50 - 200 rpm50 - 200 rpmInjection
 100 - 200 rpm100 - 200 rpmExtrusion
 
Descriptive Properties
Dynamic Service Temperature194°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENTB599 / 311292

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.