MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Epoxies, Etc 20-3035, Cat. 190 Low Density Epoxy Potting Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 20-3035 is a low density, two component epoxy potting and encapsulating system. The 20-3035 is less than half the weight of most commercially available potting compounds. 20-3035 exhibits very low shrinkage during the cure cycle and also has a low coefficient of thermal expansion. This unique epoxy system is an ideal material for the potting of electronic assemblies where a low dielectric constant and low weight are required. This epoxy syntactic foam system utilizes an advanced micro balloon technology filler. The 20-3035 provides high strength and stiffness, thermal and environmental stability, creep resistance, and water resistance. In addition to the standard bulk packaging, 20-3035 can be supplied in the ready-to-use FreezeBond® premixed and frozen syinges for elimination of waste and consistent quality.

Features:

  • Low Dielectric Constant
  • Low Coefficient of Thermal Expansion
  • Low Shrinkage
  • Low Density
  • Excellent Moisture Resistance

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.820 g/cc0.820 g/cc
Water Absorption 0.13 %
@Time 86400 sec
0.13 %
@Time 24.0 hour
Viscosity 25000 cP25000 cPMixed
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength 20.7 MPa3000 psi
Flexural Strength 48.3 MPa7000 psi
Compressive Strength 82.7 MPa12000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cm
Dielectric Constant 2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
Dielectric Strength 14.8 kV/mm375 kV/in
Dissipation Factor 0.050
@Frequency 1e+6 Hz
0.050
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 43.0 µm/m-°C23.9 µin/in-°F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.0 °C
1.00 - 2.00 hour
@Temperature 149 °F
 240 - 360 min
@Temperature 45.0 °C
4.00 - 6.00 hour
@Temperature 113 °F
 960 - 1440 min
@Temperature 25.0 °C
16.0 - 24.0 hour
@Temperature 77.0 °F
Pot Life 45.0 min
@Load 0.100 kg
45.0 min
@Load 0.221 lb
 
Descriptive Properties
Mix Ratio100:11by weight (Resin: Catalyst)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX027 / 316704

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.