Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping. Applications: gaskets, radiators, busbars, windings, switches, chemical process equipment, clad metals, printed circuit foil. Test specimens: rod - 25mm diameter. |